  "id": "YZJ-LIB-0014",
  "title": "277.14克拉浸蜡翡翠手镯：2018年荧光与FTIR记录",
  "topic": "处理与检测",
  "kind": "检测案例档案",
  "group": "knowledge",
  "summary": "这件手镯呈现强荧光，但作者并未只凭荧光把填料定为树脂。后续红外与显微观察支持重度浸蜡的案例判断。",
  "aliases": [
    "277.14克拉",
    "浸蜡",
    "FTIR",
    "强荧光",
    "Larry Tai-An Lai"
  ],
  "properties": [
    {
      "name": "报道年份",
      "value": "2018年",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "样本",
      "value": "一件绿白相间翡翠手镯",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "质量",
      "value": "277.14克拉",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "长波紫外",
      "value": "强蓝色荧光",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "折射率",
      "value": "五测点1.66",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "比重",
      "value": "3.34",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "FTIR结果",
      "value": "作者确认重度浸蜡",
      "source": "ref-yushizhijia-20260928-01"
    },
    {
      "name": "蜡相关峰",
      "value": "2850、2920、2965 cm⁻¹",
      "source": "ref-yushizhijia-20260928-01"
    }
  ],
  "sections": [
    {
      "title": "从疑点到材料判断",
      "paragraphs": [
        "荧光观察先提出需要继续检查的问题。原文记录的FTIR蜡相关结果，才对应填充物身份；不能把观察阶段的猜测替换成最后结论。"
      ]
    },
    {
      "title": "怎样保存案例分类",
      "paragraphs": [
        "档案保留2018年作者对这件样本的分类，不由此给所有经过表面上蜡的翡翠统一定性。比较另一个样本时，须重新核对对象、测试条件与实际结果。"
      ]
    }
  ],
  "facts": [
    {
      "text": "2018年Larry Tai-An Lai报道一件277.14克拉绿白手镯，长波紫外下有强蓝色荧光；五点折射率为1.66，比重3.34。FTIR分析确认重度浸蜡，蜡相关峰为2850、2920、2965 cm⁻¹；显微下见酸蚀、坑与网状裂隙。作者将该件归为B类。",
      "source": "ref-yushizhijia-20260928-01"
    }
  ],
  "fields": [],
  "steps": [],
  "limit": "仅对应报道样本，本站未检测实物；不代表中国现行标准全文结论，也不作为未知商品处理判断。",
  "sources": [
    "ref-yushizhijia-20260928-01"
  ],
  "status": "可公开知识资料",
  "authoring": "Codex资料整理与核对，未声称专业鉴定",
  "version": 1,
  "published": "2026-09-28",
  "modified": "2026-09-28",
  "checked": "2026-09-28",
  "site": "yushizhijia",
  "slug": "yzj-lib-0014",
  "url": "https://www.yushizhijia.com/library/entries/yzj-lib-0014.html",
  "image": {
    "url": "https://www.yushizhijia.com/wp-content/uploads/2026/09/knowledge-20260928-batch01/yushizhijia-01.webp",
    "width": 1280,
    "height": 800,
    "alt": "强荧光与填料身份分开：观察线索，长波紫外下强蓝色荧光，先提出检测问题；分析记录，FTIR确认样本重度浸蜡，本件并非仅凭荧光判定；适用范围，277.14克拉手镯案例，不推广到所有上蜡翡翠。原创示意，非实物照片。",
    "caption": "图：强荧光与填料身份分开。本站原创知识示意，非实物照片，不按比例。",
    "rights": "本站原创知识图解，未复制机构图片",
    "sha256": "1d077b7df62dcf63a098e6e0a8c5cadc230f6aac085fe6ef4beda43238e0dda6"
  },
  "related_entry_ids": [
    "YZJ-LIB-0002",
    "YZJ-LIB-0004"
  ],
  "related_articles": [
    {
      "title": "强荧光一定是注胶吗？277.14克拉翡翠手镯的浸蜡检测案例",
      "url": "https://www.yushizhijia.com/feicui/31995.html"
    }
  ],
  "change_reason": "新增具体研究或馆藏档案，分列对象属性、研究范围与依据。",
  "source_records": [
    {
      "id": "SRC-LIB-YUSHIZHIJIA-20260928-01",
      "title": "Strong Fluorescence in B-Jade Impregnated with Wax",
      "publisher": "GIA / Gems & Gemology；案例作者 Larry Tai-An Lai",
      "url": "https://www.gia.edu/gems-gemology/summer-2018-gemnews-strong-fluorescence-in-b-jade-impregnated-with-wax0",
      "published": "2018年夏季",
      "kind": "研究或检测案例原文",
      "summary": "2018年Larry Tai-An Lai报道一件277.14克拉绿白手镯，长波紫外下有强蓝色荧光；五点折射率为1.66，比重3.34。FTIR分析确认重度浸蜡，蜡相关峰为2850、2920、2965 cm⁻¹；显微下见酸蚀、坑与网状裂隙。作者将该件归为B类。",
      "locator": "277.14克拉手镯的观察、FTIR结果与作者案例分类",
      "scope": "仅对应报道样本，本站未检测实物；不代表中国现行标准全文结论，也不作为未知商品处理判断。",
      "checked": "2026-09-28"
    }
  ],
  "publisher": "玉石之家"
}